we do very few pfm these days (between 2-4 per month). I would love to hear some feedback on the noble and high noble SLM process. I see that Argen is doing it, anyone else? have any of you tried this? If the fits are great and the oxide layer is not too dark, it would be nice not to have to stock alloy (sorry Jensen). Thoughts?