I just kept my ears open listening to the ceramists I worked for, I hoped to be an awesome ceramist before I left for dentures.
Almost 20 higher degrees?Try this thread dentalmike knows his stuff on vita ceramics
http://dentallabnetwork.com/forums/threads/case-presentation.15936/page-5#post-162612
Yeah, monomer gives me a headache.So your dad have a fixed lab?
Not so sure about more forgiving and less headache . . .
LCM
Don't really have much monomer smell since stopped press packing. Only on hawleys or cold cure repair.Yeah, monomer gives me a headache.
But why with vita, I need to control the temperature more higher?
In the past I don't have these issues with Dental director and Noritake...and Yamamoto
ya, even the same make/model will be slightly different.All furnaces have their differences, the firing parameters from all ceramic manufacturers are guidelines for us. I do test samples and adjust my parameters no more than 5degC at a time until I find that sweet spot. Depending on the ceramic I am using then all cycles will have been adjusted either up or down from the guideline parameters.
http://imgur.com/FPQuT9k
http://imgur.com/DqzDZPC
Damn looks better
Why I need let VITA temperature higher?
I used to don't need do this with Dental director and noritake...
Is some kind of the Hard sell with VITA oven?
Experience based materials are a little bit of blind faith and a whole lot of dedication. Everyone likes things a little different.