JKraver
Well-Known Member
Full Member
- Messages
- 3,422
- Reaction score
- 451
I have heard of jet, and snap. Is there anything better, stronger, more esthetic, ect. for my dentist to use chair side on acrylic temps.
I have telios C+B material, it takes a long time to set without heat.This is one of the best cold cure tooth shaded resin I have ever used. In my opinion its an outdated material by today's standard. If I was a dentist I would use any cartridge based system if I wasn't milling in house.
http://www.ivoclarvivadent.us/en-us/products/temporary-materials/telio-product-system/telio-lab
I have telios C+B material, it takes a long time to set without heat.
Does that have the usual slime layer? Life is challenging enough without grinding scruff sticking to the slime layer while you're trying to trim temporary margins. I've never seen anything with margins more readable than good old Lang's jet acrylic and secondary decay at the poorly trimmed temp margins just plain sucks for the DDS trying to deliver the definitive and can't figure out why the margins are open. Sucks for the fixed lab who gets stuck with the remakes too.This is one of the best cold cure tooth shaded resin I have ever used. In my opinion its an outdated material by today's standard. If I was a dentist I would use any cartridge based system if I wasn't milling in house.
http://www.ivoclarvivadent.us/en-us/products/temporary-materials/telio-product-system/telio-lab
Does that have the usual slime layer? Life is challenging enough without grinding scruff sticking to the slime layer while you're trying to trim temporary margins. I've never seen anything with margins more readable than good old Lang's jet acrylic and secondary decay at the poorly trimmed temp margins just plain sucks for the DDS trying to deliver the definitive and can't figure out why the margins are open. Sucks for the fixed lab who gets stuck with the remakes too.
It says you clean the oxide layer with ethanol.Does that have the usual slime layer? Life is challenging enough without grinding scruff sticking to the slime layer while you're trying to trim temporary margins. I've never seen anything with margins more readable than good old Lang's jet acrylic and secondary decay at the poorly trimmed temp margins just plain sucks for the DDS trying to deliver the definitive and can't figure out why the margins are open. Sucks for the fixed lab who gets stuck with the remakes too.
Didn't they rename in telio.lab?Well they dont make Telio C+B anymore... anything tooth shade lab acrylic. I am considering just going back to jet.
It is light cure composite.Didn't they rename in telio.lab?