I heat to 1400 when I cast Evolution Lite, although I don't remember why.Thanks for the suggestions. Does this sound good? cold oven insert, 10 degress a min. 600 degree 30 min hold.. 50 degrees to 1550 then hold 1 hour ? I'm using Evolution Lite . 40% gold.3 turns on a Degussa manual casting machine
Understandable,,,This particular Dr. wants 40%. The patient is stage 3 with a very short life expectancy. I kinda feel a little guilty to even charge for it.I know this is a side-track to your original post...but why a high noble metal? I've found folks that need any attachments usually aren't the easiest patients on there teeth. Therefore, (and yes I've had this happen a couple times),they've broke the post or ground the attachment...hence why I'm suggesting using a base metal on these type of cast-to attachments....thoughts? agree, disagree?