R
Rugardave
Member
Full Member
- Messages
- 66
- Reaction score
- 4
WE just started using the NobleCrown metal froma Argen, Both from a different lab and our own. On frames from both labs we have gotten little bubbles coming out of the porc. We normally use the 76SF and have never had this prob. Is this par for the course? or is it something we are doing. Both places have conditioned the metal by the book. I have talked to techs from the com. and others that sell the metal under their own name. WE follow directions to the T and Still have this problem. Not all the time, but sometimes on units out of the same ring. Singles and bridges. We finish we crosscut carbides.
Who's had this problem and what did you do the eliminate it? Or should we say screw it and go back the something we know.
Thanks, R. Dave
Who's had this problem and what did you do the eliminate it? Or should we say screw it and go back the something we know.
Thanks, R. Dave