I need to have a very long burnout cycle for the 3D modeling patterns We use. The manufacturer recommends 500 insertion , 15 degrees a minute to 800 , hold for 30 minutes, 15 deg/min. to 1600 hundred and then a hold of at least one hour.
I would like to put my rings in a cold furnace before going home for the night and have my rings ready to cast or press shortly after I get in. I am using Galaxy II from Talladium. Having no experiece doing this I am concerned about cracked rings. Any and all help would be appreciated.
I would like to put my rings in a cold furnace before going home for the night and have my rings ready to cast or press shortly after I get in. I am using Galaxy II from Talladium. Having no experiece doing this I am concerned about cracked rings. Any and all help would be appreciated.