remember that each furnace gives different temp. So you can start with these parameters and adjust them to your demands. I sometimes press for less than 10 min . And still get good results.but temp not less than 917 C.
Want to minimize that reaction layer? Minimize those pressing times, how?....ease that pressing temp up . No time to test? Bettter than trying to find time to re-press a case that is really due.