Any one doing these routinely with systems like medentibase or Renishaw laser abutments?
I'm looking to try one piece designs with direct ceramic build up as I'm tired of sticking units to ti interfaces. But if the interface is in chrome cobolt and given past experience of trialling slm chrome cobolt and the horrid oxide that it produces, doesn't the oxide and subsequent cleaning completely screw the interface?
maybe the medentibase approach produces less issue then slm as the interface is pre milled and not slm?
I'm looking to try one piece designs with direct ceramic build up as I'm tired of sticking units to ti interfaces. But if the interface is in chrome cobolt and given past experience of trialling slm chrome cobolt and the horrid oxide that it produces, doesn't the oxide and subsequent cleaning completely screw the interface?
maybe the medentibase approach produces less issue then slm as the interface is pre milled and not slm?