Long story short. Straumann deleted a file I submitted a wile ago and now I don't want to start over but may have to. By chance does anyone know of a place that mills BLX custom abutments other then straumann?
Any idea why 6 milled emax units would grey out during sintering ? I've sintered other units after that came out fine. Are these salvageable? I sinter everything the same. same pegs, same putty, same trays.
Some of my implants can't be anodized so I am going to do it my self. Now the question is I understand the voltage needed has to be 100 or more. Does the Amps matter as well?
Rick
Has anyone dealt with Apha bio internal hex? Can it be crossed referenced with another system? Client has a patient who needs one that needs a new crown. Problem with the abutment is that it is to far sub g to capture margin correctly.
Rick
Trying to learn about which resins you guys like the best for models and wax up's? Are there any resins that can be used in rapid burn out? I have read about Form labs and asiga, Just wanted to see what others might be using and why such as the lower shrinkage, ease of post processing and so...
Which resins do you find give you the most accuracy for digital models and crown and bridge? Is there a resin that can be case in the rapid burnout technique. Is the post processing alcohol only or do you need a light cure as well.
Years ago I was conversing with Dr Niznick at one time and he stated that his parts had a tolerance of 1% vs name brand that had a 3% tolerance. He also said he saw no need for Ti bases either ; }
Got a good lab doing my milling for some time now. I have been having the occasional loose fit of my zirconia to ti bases. 2 were using tru abutments scan bodies ( nobel trilobe and 3i) and a 3rd was using a glidewell scan body (nobel) . Know one seems to know the answer. Anyone have a suggestion?