Forums
New posts
Search forums
What's new
New posts
Latest activity
Articles
Members
Current visitors
Log in
Register
What's new
Search
Search
Search titles only
New posts
Search forums
Menu
Log in
Register
Install the app
Install
Forums
Lab talk, the good, the bad, and the ugly
Metal
Up charge on alloy's....
JavaScript is disabled. For a better experience, please enable JavaScript in your browser before proceeding.
You are using an out of date browser. It may not display this or other websites correctly.
You should upgrade or use an
alternative browser
.
Reply to thread
Message
<blockquote data-quote="dmonwaxa" data-source="post: 164019" data-attributes="member: 927"><p>For ex lets assume:</p><p> </p><p>Alloy wt prior to melting =15.7</p><p>button after casting =15.3</p><p>(casting loss = .4)</p><p>button prior to despruing =15.3</p><p>button after despruing =6.8</p><p>desprued castings weight =7.9</p><p>button + castings (6.8 + 7.9) =14.7</p><p>despruing loss=(init wt -casting loss -button - castings)(15.7 -.4 -6.8 -7.9)= .6</p><p>Total loss = 1.0g</p><p> </p><p>or another way = init wt - (casting loss + despruing loss + castings wt)</p><p> = 15.7 - ( .4 + .6 +7.9)</p><p> = 15.7 - (8.9)</p><p>button wt (on hand) = 6.8 g </p><p>Alloy used for castings= init alloy wt -button wt(15.7-6.8) =8.9</p><p> </p><p>bottom 2 lines should add up to initial wt</p></blockquote><p></p>
[QUOTE="dmonwaxa, post: 164019, member: 927"] For ex lets assume: Alloy wt prior to melting =15.7 button after casting =15.3 (casting loss = .4) button prior to despruing =15.3 button after despruing =6.8 desprued castings weight =7.9 button + castings (6.8 + 7.9) =14.7 despruing loss=(init wt -casting loss -button - castings)(15.7 -.4 -6.8 -7.9)= .6 Total loss = 1.0g or another way = init wt - (casting loss + despruing loss + castings wt) = 15.7 - ( .4 + .6 +7.9) = 15.7 - (8.9) button wt (on hand) = 6.8 g Alloy used for castings= init alloy wt -button wt(15.7-6.8) =8.9 bottom 2 lines should add up to initial wt [/QUOTE]