Forums
New posts
Search forums
What's new
New posts
Latest activity
Articles
Members
Current visitors
Log in
Register
What's new
Search
Search
Search titles only
New posts
Search forums
Menu
Log in
Register
Install the app
Install
Forums
Lab talk, the good, the bad, and the ugly
Zirconium
Staining "up" Pre-shaded Zirconia and D and C shades
JavaScript is disabled. For a better experience, please enable JavaScript in your browser before proceeding.
You are using an out of date browser. It may not display this or other websites correctly.
You should upgrade or use an
alternative browser
.
Reply to thread
Message
<blockquote data-quote="Affinity" data-source="post: 306171" data-attributes="member: 1246"><p>Order some changs ilquids. I never understood preshaded zirconia.. Who has the time to group units together by color and change pucks but not to color them by hand? It takes less than 20 seconds to color a crown. Theres no gradient in a preshaded puck, just monotone. </p><p></p><p>You can of course stain preshaded zirconia, but at that point, why not just mill white and control the color from a blank slate? </p><p>NexxzrT is good for posteriors, not as nice looking obviously, chalky, but tough as a mother.</p></blockquote><p></p>
[QUOTE="Affinity, post: 306171, member: 1246"] Order some changs ilquids. I never understood preshaded zirconia.. Who has the time to group units together by color and change pucks but not to color them by hand? It takes less than 20 seconds to color a crown. Theres no gradient in a preshaded puck, just monotone. You can of course stain preshaded zirconia, but at that point, why not just mill white and control the color from a blank slate? NexxzrT is good for posteriors, not as nice looking obviously, chalky, but tough as a mother. [/QUOTE]
Insert quotes…
Verification
Who do we work for?
Post reply
Forums
Lab talk, the good, the bad, and the ugly
Zirconium
Staining "up" Pre-shaded Zirconia and D and C shades
Top
Bottom