Forums
New posts
Search forums
What's new
New posts
Latest activity
Articles
Members
Current visitors
Log in
Register
What's new
Search
Search
Search titles only
New posts
Search forums
Menu
Log in
Register
Install the app
Install
Forums
Lab talk, the good, the bad, and the ugly
Zirconium
Finishing Zir. Bruxer crs
JavaScript is disabled. For a better experience, please enable JavaScript in your browser before proceeding.
You are using an out of date browser. It may not display this or other websites correctly.
You should upgrade or use an
alternative browser
.
Reply to thread
Message
<blockquote data-quote="DMC" data-source="post: 44174" data-attributes="member: 430"><p>My wife adds anatomy if it does not look like a tooth out of the mill with a high speed NSK and needle point bur BEFORE stains and sintering. Very light touch. </p><p></p><p>That's the only way you are going to make it look like a PFM.</p><p></p><p>Never seen a mill with a needle point bur doing the secondary anatomy ONLY, but I'm sure it will happen one day.</p><p></p><p>Zirconia is too hard to do this in the green state. You will get burnt Grey metal all over the Occlusal, or go broke in diamond point burs.</p></blockquote><p></p>
[QUOTE="DMC, post: 44174, member: 430"] My wife adds anatomy if it does not look like a tooth out of the mill with a high speed NSK and needle point bur BEFORE stains and sintering. Very light touch. That's the only way you are going to make it look like a PFM. Never seen a mill with a needle point bur doing the secondary anatomy ONLY, but I'm sure it will happen one day. Zirconia is too hard to do this in the green state. You will get burnt Grey metal all over the Occlusal, or go broke in diamond point burs. [/QUOTE]
Insert quotes…
Verification
Who makes the popular shade guide?
Post reply
Forums
Lab talk, the good, the bad, and the ugly
Zirconium
Finishing Zir. Bruxer crs
Top
Bottom