Forums
New posts
Search forums
What's new
New posts
Latest activity
Articles
Members
Current visitors
Log in
Register
What's new
Search
Search
Search titles only
New posts
Search forums
Menu
Log in
Register
Install the app
Install
Forums
Lab talk, the good, the bad, and the ugly
Zirconium
Zirconia testing
JavaScript is disabled. For a better experience, please enable JavaScript in your browser before proceeding.
You are using an out of date browser. It may not display this or other websites correctly.
You should upgrade or use an
alternative browser
.
Reply to thread
Message
<blockquote data-quote="millennium" data-source="post: 343536" data-attributes="member: 13239"><p>I had the same experience with zirlux transitions, I sintered at 1480 as they suggest results were very little chroma and translucency. I tried from 1400 to 1500, same outcome.</p></blockquote><p></p>
[QUOTE="millennium, post: 343536, member: 13239"] I had the same experience with zirlux transitions, I sintered at 1480 as they suggest results were very little chroma and translucency. I tried from 1400 to 1500, same outcome. [/QUOTE]
Insert quotes…
Verification
Who do we work for?
Post reply
Forums
Lab talk, the good, the bad, and the ugly
Zirconium
Zirconia testing
Top
Bottom