Forums
New posts
Search forums
What's new
New posts
Latest activity
Articles
Members
Current visitors
Log in
Register
What's new
Search
Search
Search titles only
New posts
Search forums
Menu
Log in
Register
Install the app
Install
Forums
Lab talk, the good, the bad, and the ugly
Zirconium
Sintering Zirconia Q&A
JavaScript is disabled. For a better experience, please enable JavaScript in your browser before proceeding.
You are using an out of date browser. It may not display this or other websites correctly.
You should upgrade or use an
alternative browser
.
Reply to thread
Message
<blockquote data-quote="spokas" data-source="post: 191471" data-attributes="member: 10105"><p>Could anyone answer what i did wrong. I have kerox zirkonia ant mihm vogt ht-s speed sintering furnace. If Im using kerox recomended parameters my restorations usually are too narrow so I started using metoxit parameters and everything is fine. My kerox zirkonia sintering parameter:</p><p>s1 10 900 30</p><p>s2 5 1450 120</p><p>s3 10 900 0</p><p>s4 10 150 0</p><p>metoxit parameters:</p><p>s1 2 300 15</p><p>s2 5 1500 60</p><p>s3 10 900 0</p><p>s4 10 300 0</p><p></p><p>thanks</p></blockquote><p></p>
[QUOTE="spokas, post: 191471, member: 10105"] Could anyone answer what i did wrong. I have kerox zirkonia ant mihm vogt ht-s speed sintering furnace. If Im using kerox recomended parameters my restorations usually are too narrow so I started using metoxit parameters and everything is fine. My kerox zirkonia sintering parameter: s1 10 900 30 s2 5 1450 120 s3 10 900 0 s4 10 150 0 metoxit parameters: s1 2 300 15 s2 5 1500 60 s3 10 900 0 s4 10 300 0 thanks [/QUOTE]