B
BruceQuality
New Member
- Messages
- 47
- Reaction score
- 0
I posted this over in the porcelain forum, then thought it might fit here too, so sorry ahead of time for duplication.
We are experiencing a problem with our Finesse paste opaques (just a few) bubbling when a porcelain shoulder is being added to the opaqued coping on EDITED, Silhouette Line, 250 SL, (74.78% Palladium.) Has anybody else experienced this? Did you find a remedy if so?
The shades we are experiencing this with are: A0, A2, A3, A4, B1, C1 and D4.
Our opaguing technician worked in another lab a few years ago and experienced the same difficulty with their silver palladium (different metal than ours.) So we now know that this is not an isolated issue and it began before she arrived, so it is not isolated to any individual in the lab either.
Thanks for any/all input!
We are experiencing a problem with our Finesse paste opaques (just a few) bubbling when a porcelain shoulder is being added to the opaqued coping on EDITED, Silhouette Line, 250 SL, (74.78% Palladium.) Has anybody else experienced this? Did you find a remedy if so?
The shades we are experiencing this with are: A0, A2, A3, A4, B1, C1 and D4.
Our opaguing technician worked in another lab a few years ago and experienced the same difficulty with their silver palladium (different metal than ours.) So we now know that this is not an isolated issue and it began before she arrived, so it is not isolated to any individual in the lab either.
Thanks for any/all input!
Last edited: