Forums
New posts
Search forums
What's new
New posts
Latest activity
Articles
Members
Current visitors
Log in
Register
What's new
Search
Search
Search titles only
New posts
Search forums
Menu
Log in
Register
Install the app
Install
Forums
Lab talk, the good, the bad, and the ugly
All Porcelain-Press
Help, new to pressing
JavaScript is disabled. For a better experience, please enable JavaScript in your browser before proceeding.
You are using an out of date browser. It may not display this or other websites correctly.
You should upgrade or use an
alternative browser
.
Reply to thread
Message
<blockquote data-quote="Drews Dental Lab" data-source="post: 339284" data-attributes="member: 22621"><p>I changed my hold time to 25 min and this is my result, The glossy areas are from me trying to see how far the pitting went. Fit was good just pitting and rough margins.</p><p></p><p>Microstar investment </p><p></p><p>Lisi</p><p>Whip mix SP</p><p>Conventual Press </p><p>700 entry</p><p>60 rise</p><p>860 hold temp</p><p>14 min hold time</p><p>8 min press</p><p>2 min cool</p><p></p><p>67 psi</p></blockquote><p></p>
[QUOTE="Drews Dental Lab, post: 339284, member: 22621"] I changed my hold time to 25 min and this is my result, The glossy areas are from me trying to see how far the pitting went. Fit was good just pitting and rough margins. Microstar investment Lisi Whip mix SP Conventual Press 700 entry 60 rise 860 hold temp 14 min hold time 8 min press 2 min cool 67 psi [/QUOTE]