JavaScript is disabled. For a better experience, please enable JavaScript in your browser before proceeding.
You are using an out of date browser. It may not display this or other websites correctly.
You should upgrade or use an
alternative browser
.
Reply to thread
Message
<blockquote data-quote="Drews Dental Lab" data-source="post: 339159" data-attributes="member: 22621"><p>Here is my result after increasing to 865c and increasing to 10 min hold time also with 67 psi </p><p></p><p>Still a little pitted I don't know if that normal/acceptable and my sprue angle could be better</p></blockquote><p></p>
[QUOTE="Drews Dental Lab, post: 339159, member: 22621"] Here is my result after increasing to 865c and increasing to 10 min hold time also with 67 psi Still a little pitted I don't know if that normal/acceptable and my sprue angle could be better [/QUOTE]