Chipped PFM

McTeeth

McTeeth

Active Member
Donator
Full Member
Messages
335
Reaction score
37
Hey Everyone,

I had a Dr contact me regarding ideas on how to attach chipped feldspathic back onto a long PFM bridge (crown #13). He attempted x2 to bond it but it keeps coming off. I said I will ask around, I even said maybe Krazy Glue?? Dontknow.

Anyone have some fancy pants ideas?
Thanks,
Sean
 

Attachments

  • PFM.jpg
    PFM.jpg
    49 KB · Views: 40
C

charles007

Well-Known Member
Full Member
Messages
3,828
Reaction score
453
Ask doctor to prep the buccal and carry over part of occlusal with no undercuts for pfm, will last forever, Waxed many of these over the years on poorly supported pfm frames but usually on anteriors with 3mm of chipped off porcelain. :rolleyes:
Sorry, use to have a saved model to show doctors how to prep. Maybe someone can post up a picture !
 
D

Dentalmike

Well-Known Member
Full Member
Messages
187
Reaction score
140
I’ve done fixes in the past for this by the doc doing taco shape prep ( cover facial/lingual leaving proximals mostly in tact) usually in a pontic area to save removing an entire bridge.
 
2thm8kr

2thm8kr

Beanosavedmysociallife
Full Member
Messages
11,246
Reaction score
2,510
I’ve done fixes in the past for this by the doc doing taco shape prep ( cover facial/lingual leaving proximals mostly in tact) usually in a pontic area to save removing an entire bridge.
Yes, but be sure to charge more that street taco prices for bailing out a large bridge case that ultimately should be redone.
*Edit to add Krazy Glue/cyanoacrylate is biodegradable. It will work for a time, but then you're wishing for tacos again. 🌮🌮🌮🌮🌮
 
rkm rdt

rkm rdt

Well-Known Member
Full Member
Messages
18,708
Reaction score
3,288
Yes, but be sure to charge more that street taco prices for bailing out a large bridge case that ultimately should be redone.
*Edit to add Krazy Glue/cyanoacrylate is biodegradable. It will work for a time, but then you're wishing for tacos again. 🌮🌮🌮🌮🌮
I think the idea here is to let the cyanide finish the job.
 