Gold (AU) 72
Platinum (PT) 13.9
Palladium (PD) 0
Silver (AG) 10.5
Copper (CU) 0
Zinc (ZN) 3

Anybody have any experience using this metal? It looks like a good alternative for me. I've used Argelite 75+6 for pfm crowns for many years, but palladium prices have gone insane lately.
 