I'm thinking about moving to Canada or USA
And I have some questions about dental laboratory trade market there.
My friend told me, that his career is down and down thanks to china laboratories invasion to US
and too many technician leaving there jobs and looking to another career
Any body...
I have a problem with the thrmoplastic material of vertex
we get new system Thermosens and do as in training video
we using sand paper ,silicon polisher and pumice
but it still show the coarse surface with poor shiningDontknow
any body have useful way to do it so well
I've made long bridge with a sigficant curving
using ZirkonZahn system
but when I order to make stablizer it show outside the curve
ist normal ?? I am afraid it could distruct the counstruction
hey
I had made an 8 unit bridge by using prettau blanck of zirconzahn
after I finished the glaze circle it broken into tow pieces :mad::mad::mad: !!!
I made it again but it broken in the same area during finishing the zirconia
:frusty:
plz tell me what is the problem :hail...
hey
I need more information about lumineers
can we make it by zirconia ??
I have CAD/CAm system and the doctors are asking me about it!:confused::confused:
I recive a case of old patient and my dentist ask me to mak avirtual crack among the pfm crn (vita VMK95) to match proximal teeth I haven't done before please I need help with photos if possible How to make it:confused::confused::confused:.
thanks