Hello,
I can only tell you my experience with 5 by 400 , I’m not familiar with the other mill. I only mill around 250 zirconia units per month, but I believe you can mill Zirconia all day long. I change my water tank and clean the collet once a week. Always use good burs and don’t go over...
Hi fusing is a whole different animal . It handles differently as well . I just use it as a skin layer . You can polish it afterwards. You have to be pretty precise though
What’s worked for me is using glaze liquid only and Miyo on first bake. Wet your restauration with glaze liquid , apply Miyo. Drying time is 10-12 minutes , I don’t remember exactly. Then do a glaze bake for the second bake . Nowadays I use structure hi fusing after first bake , i do the final...
Sometimes my doctors use Creodent scan bodies and I design the whole thing , abutment , crown , dim model and I send out the abutment and model and do the crowns in house. I’m sure on those type of cases I have to set the annotation. Who knows anymore? Leave it to high tech to screw up something.
I get core files from encode cases and a lot of times I have to adjust for that . Those are all IOS . So , they design the abutment , I check it and then I get a core file that I use to design my crown from.