  1. D

    Verification jig

    Hi everyone does anyone know where can I found stone 0% expansion for verification jigs. I’m doing my verification jigs with gc pattern recin but it’s flexible and I have sometimes problems. If somebody knows a different technique that might work pls Feel free to tell me
  2. D

    Black zirconia

    Hi guys does anyone knows why these happened? It's zirconia framework with czr layered on top on the6 anterior.everything went fine until the time I glazed. I glazed the raw zirconia with emax glaze and where I put emax glaze it turned black. I sandblasted the black places and I got the black...
  3. D

    Verification jigs?

    Hi to all. I have 2 questions that i would like to hear your thoughts . First is which material do you guys use for verification jigs for full arch implant restoretions. Im using gc pattern resin but i think that is to flexible and tolerant so mistakes might happened. Ive heard about stone...
  4. D

    Hybrids and materials to use

    Hey guys I want to say some thoughts about choosing material for a hybrid and I would love to hear your thoughts and opinions about that. I'm an inlab technician and lately at the clinic we have a few cases over implants for hybrid design. The last hybrid that we did was with PEEk material...
  5. D

    Implant scan bodies in exocad library

    Need help figuring out what scan bodies in my medit hybrid cad library for Nobel replace conical connection and stray man cc. What are the codes/ abbreviations in this library for these platforms. Sent from my iPad using Tapatalk
  6. D

    Polishing techniques

    Hey guys need help again. I m doing some full occlusal non precious and precious crown and im having problem on polishing the grooves does anybody knows any websites to recomend for buying burs and rubbers and if yes which one do you suggest. If there are any special techniques on how to polish...
  7. D

    Casting non precious on ucla abudment with precious base?

    A question again if you can help im using semi only because i cast nobel implants castable that has precious base. People told me that they use a non precious metal to cast and they dont have problems of merging the two metals. Do anybody know anything. I dont want to use semi precious any more...
  8. D

    Porosity on semi precious

    Hi guys i m doing a semi presious alloy( for the first time)cerapall 6 and im using EX3 noritake . I did oxidation but on the first opague it was full of porosity can somebody give me any advice
  9. D

    Casting gold

    Hi guys A dr of mine wants to start casting gold. I have to buy a new scale but from a search that i did the prices are from 50 euros up to 800 euros. What is the diferrence and there are these big diferences, are the more expensive more accurate? Im gonna be weighing wrong without knowing and...
  10. D

    PROBLEM PLS HELP

    Hi guys. I want the groups help or advice. I have medit identica hybrid scanner and yesterday i scanned a bridge and when i reached at the die scanning part for the first time the scanned dies looked weird. Ill put a pic to show what i mean but to descriped it it was like broken pixels on some...
  11. D

    Looking for a small induction casting machine

    Hey guys, Need some recomendations for a small induction casting machine. Im in a 2 man lab and have a need for basic crown and bridge castings. Would like to have a low maintanance machine with minimal needs for it to run. Its my first one so i have no idea of the different kinds (ie gas or...
  12. D

    Sam 2PX articulators

    Does anyone has a sam 2PX for sale and how much Sent from my iPad using Tapatalk
  13. D

    Medit scanner

    Hey there i m interested in buying the identica scanner from medit. Anyone uses it or knows any infos on any of their models? I want to know the good and the bad between the models (hybrid,blue ,light)and if someone think is not reliable any other suggestions? Thanks Sent from my iPad using...
  14. D

    Want to buy a cad cam

    Hi guys im interesting in buying a cad cam. I dont know anything about cad cams but i know that is the future. Can you suggest something or give me some directions like what is important for a scanner to have or a milling machine so i can look up for that
  15. D

    Green on metal

    Hi guys i have an issue and i need your advice. When i finish my porcelain the metal from the inner side of the crown gets a thin layer of green. I always sand blast my work at the and so that the green layer disappear. Does that green layer affect the cementation? If yes how can i get reed of...
  16. D

    Best system for wax?

    Hi guys i would like your opinion on what system do you reccomend for the waxing of bridges( accu track pin dex dentona .............)any sujestions? Sent from my iPad using Tapatalk
  17. D

    Bridge difference in mouth

    Hi everyone im using the accu track system. When i do my casting i see that on the accu track im ok. I then make another model without using any system to check if im ok. Ive notice many times that im ok on the accu track but on the cast( immobilize cast didnt used any system) the bridge doesnt...
  18. D

    Porocity on opaque

    Hi my friends im using the classic porcelain and lately i have a porocity problem when i do opaque. Does anybody have any ideas to help?
  19. D

    red spot on emax

    Hi ive made 6 veneers on the maxilla from canine to canine. i used emax LT ingot. 2 months after the cementation on the cervical area of one of the canine a red brown spot appeared. does anybody knows why that happened and if there is a solution how that can go away?