So, Ivoclar came out with new firing parameters for e.max ceram on LS2 and ZrO2. It is a two stage firing and the end temperature is lowered by 20 degrees... I tried it on a couple crowns, today. And yes, I still layer anteriors, and will so for a while... . Anyway, I actually 'think', I can feel a difference in surface quality. I would like to know what brought them to do that, after e.max being on the marked for more than 10 years, already...