Search results

  1. Gdentallab

    Milling and casting polymer ...

    NiCr will . But CrCo will not.
  2. Gdentallab

    Most used investment for emax?

    sliadent. precision, fast, strong(never had a ring cracked) and yet very very easily divested. siladent premium, it can be used for metal as well.
  3. Gdentallab

    Restorations Du Jour

    Yes all pfz . Zirconzahn (so far I'm getting best results ) . And GC ceramic. In fact I'm not completely satisfied with the lines & contour ! :) i got to learn and practice more ! But overall I'm satisfied .
  4. Gdentallab

    Restorations Du Jour

    full upper hello,
  5. Gdentallab

    Restorations Du Jour

    upper zirconia hello,
  6. Gdentallab

    All things GC Initial

    what opaque are you using, powder or paste? I just love the powder but its liquid is not as i expect. GC is known for the clf . Clear fluo. Do you use it a lot ? How about the enamel occlusal 15 , 16 , 17 . I just love them.
  7. Gdentallab

    All things GC Initial

    Affinity what insides you got and how do you use them ? It's been two years I'm on GC . Mc . Zr . And IQ . Its great. The reflective light kit can be used to change the shade of Zr core after sintering.
  8. Gdentallab

    porosity in gold bridge

    i know it's against all what we studied and most of the education, but sprues on the pontic makes porosity , so why not eliminate the sprues on the pontics? it really works fine , even for full bridge with a large number of pontics.
  9. Gdentallab

    Nondas Vlachopoulos Course, 6/7 April in Athens

    it would be great ! But my wife will be delivering at that time .! What shall i do ? I love Athens and don't wanna miss NONDAS!
  10. Gdentallab

    Restorations Du Jour

    Al your teeth are alive !!!!!!!!!!! so beautiful. you should sue those low @rses!!!!!!!!!
  11. Gdentallab

    Pink porcelain

    GC have pink porcelain kit . Gum shade kit
  12. Gdentallab

    Finesse firing chart?

    Powder opaque finesse: 3min dry, 3 min preheat, start temp 450 C, heat rate 90 C, final temp 800 C. full vacuum. paste opaque finesse: 5 dry , 3 preheat, start 450 heat rate 90 C , final 790 , full vacuum. dentine: 5 min dry, 5 min preheat, heat rate 35C/min , final temp 760 C.firing time 30...
  13. Gdentallab

    FaceBook postings

    nice, interesting.
  14. Gdentallab

    Emax Staining

    if you have the lustre paste, you should try the V , value paste it will elevate the value somehow. why not try it. paste V on all the crown, and add some L1 vanilla on the incisal . give it a try.
  15. Gdentallab

    Quiet Vacuum Pump

    there's vacuum pumps that run on oil, it comes with the touch n press. though it needs maintenance (changing oil) but it is very silent and durable. Doug, you put your kids in a box !!!! :peep: :D
  16. Gdentallab

    expert in cad

    Is there an academy, school, or university to become let's say expert in cad software. How can we know the benefits of each system, the tricks, how to deal with each situation? should i take all available courses? should i get a toy( cad cam) and play with it? i don't own any cad cam, had a...
  17. Gdentallab

    fracture in FC zirconia

    I think the price of gold is somehow the same everywhere. you'd rather ask how much the technician delivers the restoration (gold or Zr) to his account...
  18. Gdentallab

    Amann Girrbach Giroform model system

    Drizzt, i actually can't answer you because i haven't tested zeiser or giroform. we need someone who have both systems to compare.
  19. Gdentallab

    Amann Girrbach Giroform model system

    i find the giroform expensive, why not use a system such as SILADENT Dr. Böhme & Schöps GmbH - Products very fast , not expensive, and i believe the end result is similar, it's been a year i'm using it, very satisfied. i still use the pindex, some old techniques never die. :)
  20. Gdentallab

    Restorations Du Jour

    you're right, they look grainy. dunno why!
Top Bottom