Very interesting stuff on d.sign,
Steam Tears = lower the intial heat temp. (Tony) OR get rid of the dry time (Brian)
Bridges= always seperate (Tony)

Currently, I use Finesse (Dentsply, getting rid of it within two weeks), D.Sign (Ivoclar), Avante (Pentron), E.max (Ivoclar), Esthetic (Ivoclar). I wanna try the Noritake system because of the price, so hopefully in the future I will.

My favorite is D.Sign, because I'm a color whore, you throw that on a Captek crown you won't find better chroma, hue, and value. It can be a *bleep* to work with sometimes, but hopefully some of the tricks above will help out with some of the tearing.