I use HN. W, from Ivoclar 54% au. Also I use Brite Gold 96.3% au (BG XH 88.9%for bridges) as a replacement to captec. Glass bead the inside and you cant tell the difference between the two.
One thing I dont like is to use an alloy like some high PD types that require you to sand blast after oxidation.
Higher prices isnt really a factor for me because its been an incentive for Drs to use all ceramic.
Also I love the return on the scrap!!!!